Surface Roughness of Restoration Margin Preparations: A Comparative Analysis of Finishing Techniques
Warning: include(/home/quintpub/public_html/journals/prdincludes/05_update/javascript.php) [function.include]: failed to open stream: No such file or directory in /home/quintpub/public_html/journals/prd/abstract.php on line 39

Warning: include() [function.include]: Failed opening '/home/quintpub/public_html/journals/prdincludes/05_update/javascript.php' for inclusion (include_path='.:/usr/lib/php:/usr/local/lib/php') in /home/quintpub/public_html/journals/prd/abstract.php on line 39
Follow Us      

LOGIN

   Official Journal of The Academy of Osseointegration

 
Share Page:
Back

Volume 35 , Issue 2
March/April 2015

Pages 211-218


Surface Roughness of Restoration Margin Preparations: A Comparative Analysis of Finishing Techniques

Isabelle Clarke, BSc, BDent/Adriana Aquilia, BSc, BDent/Luiz Eduardo Bertassoni, DDS/Massimiliano Guazzato, DDS, DClinDent, PhD/Iven Klineberg, BSc, MDS, PhD


PMID: 25738341
DOI: 10.11607/prd.1829

This study compared the margin profile and surface roughness created by the tips of four different finishing instruments: fine diamond, dura white stone, tungsten carbide, and ultrasonic diamond-coated tips (UDTs). The aim was to determine which of these instruments produced the smoothest finish and created the most evenly contoured margin characteristics. It was hypothesized that UDTs would produce a rougher dentin surface than a fine diamond bur, that a tungsten carbide bur would provide a smoother finish than a fine diamond, and that the dura white stone would produce an intermediate finish. Forty extracted premolars were divided into two groups. For the first group, a 1.5 x 3.0-mm dentin slot was prepared in 30 teeth using a control 50-μm diamond bur, followed by one of the four finishing instruments. The surface roughness (Ra) was then measured using a surface profilometer and a one-way analysis of variance followed by a post hoc Bonferroni test to assess whether any statistical difference existed among the Ra values. For the second group, shoulder margins were prepared in 10 teeth. They were then refined with one of the four finishing instruments and examined with scanning electron microscopy (SEM). The fine diamond bur created a significantly smoother surface than the control diamond (P < .001), UDTs (P < .007), and tungsten carbide bur (P < .010). The fine diamond was not found to be significantly smoother than the dura white stone. SEM images of the fine diamond showed divoting on the margin floor. The dura stone showed a well-defined, undamaged margin. The tungsten carbide bur created frequent chipping in enamel margins. The UDT specimens showed an inconsistent finish and discrete patches of open dentinal tubules. The fine diamond created the lowest Ra values; however, the dura stone offered efficient finishing and less damage to the margin profile.


Full Text PDF File | Order Article

 

 
Get Adobe Reader
Adobe Acrobat Reader is required to view PDF files. This is a free program available from the Adobe web site.
Follow the download directions on the Adobe web site to get your copy of Adobe Acrobat Reader.

 

© 2020 Quintessence Publishing Co, Inc

PRD Home
Current Issue
Ahead of Print
Archive
Author Guidelines
About
Submission Form
Submit
Reprints
Permission
Advertising
Quintessence Home
Terms of Use
Privacy Policy
About Us
Contact Us
Help